Description Features 7-inch TFT Colour display High precision crack & weld detection Operating frequency up to 20 MHz Velocity range: 100 to 20,000 m/s High sensitivity ≥65 dB Dynamic range ≥35 dB Large data storage (up to 20,000 sets) Wireless cloud data transmission (optional) Lithium battery power supply Portable and durable engineering plastic body Technical Specifications Parameter Value Testing Range 0 to 15,000 mm (0 to 590.55 in) Working Frequency 0.5 to 20 MHz Gain 0 to 110 dB Reject 0 to 80% Probe Type Single, Dual, Through, Immersion type